The cross-direction (transverse) ring crush index test is the primary method for evaluating the edgewise compression performance of corrugating medium, the fluted layer that largely determines the stacking strength of corrugated boxes. Performed in accordance with ISO 12192 and GB/T 2679.8, the test converts the maximum ring crush force into a grammage-normalized index expressed in N·m/g, allowing fair comparison between papers of different basis weights. This article explains the test principle, specimen requirements, apparatus, calculation procedures, and industrial applications of the transverse ring crush index test for corrugating medium.
Technical Overview
Corrugating medium, also known as corrugated base paper or fluting, is the fluted middle layer of corrugated board that provides rigidity, cushioning, and vertical load-bearing capacity to shipping containers. Because the medium carries a significant share of the compressive load when a box is stacked, its edgewise compression performance is one of the most important quality indicators in the containerboard supply chain.
The ring crush test measures the resistance of a narrow paper strip to edgewise compression. A specimen strip is curled into a circular ring and held in a precision ring holder, which supports the long edges while a controlled length of the ring is crushed between two parallel platens of a compression tester. The maximum force sustained before collapse is recorded and converted into ring crush strength, expressed in kN/m.
For corrugating medium, the test is specifically performed in the cross-machine direction (transverse direction, CD). The reason is geometric: during the corrugating process the flute axes run parallel to the machine direction of the paper, so when the finished board is loaded vertically the medium carries the load as a series of arches oriented in the paper's cross direction. Consequently, the transverse ring crush index of the medium correlates strongly with the edgewise crush strength (ECT) of corrugated board and, through empirical models such as the McKee formula, with the ultimate box compression strength.
Because heavier papers naturally resist more force, the ring crush strength is normalized by grammage to obtain the ring crush index, expressed in N·m/g. This index allows mills, converters, and buyers to compare the intrinsic compression quality of medium across different basis weights. The test is governed by the following key standards and reference documents:
- ISO 12192, Paper and board — Determination of compressive strength — Ring crush method
- GB/T 2679.8, Chinese national standard for the determination of ring crush strength of paper and board
- GB/T 13023, Chinese national product standard for corrugating medium, which specifies minimum transverse ring crush index requirements by grade
- ISO 187 / GB/T 10739, standard conditioning atmospheres for testing paper and board
- ISO 186 and ISO 536, sampling and grammage determination used to support the index calculation
Testing Samples
Corrugating Medium (All Commercial Grades)
The test applies to corrugating medium of all commercial grades, including ordinary recycled medium, semi-chemical medium, and high-strength medium produced from virgin or blended furnish. Common basis weights range from approximately 90 g/m² to 200 g/m², with 110 g/m², 120 g/m², 140 g/m², and 170 g/m² being widely traded specifications. The method is equally applicable to pilot-scale handsheets and machine-made reels, provided that the specimens are representative of the lot.
Specimen Requirements
Specimens are narrow strips cut with clean, parallel edges and free from wrinkles, water marks, creases, or visible defects. The standard specimen is approximately 12.7 mm wide and 152 mm long, matching the circumference of the standard ring holder. The following requirements are typical:
- A minimum of ten valid strips cut in the cross-machine (transverse) direction, taken from at least five different positions distributed across the reel or sheet web width
- Cut edges sharp and parallel, without burrs or fuzz that could affect seating in the holder
- Strips must not be bent, folded, or contaminated by handling, and should be identified by direction and position
- Matched specimens reserved for grammage determination in accordance with ISO 536
Sample Conditioning
Before testing, all specimens must be conditioned to equilibrium in the standard atmosphere of 23 °C ± 1 °C and 50 % ± 2 % relative humidity as defined in ISO 187 (equivalent to GB/T 10739), normally for at least 24 hours. Paper compression properties are highly sensitive to moisture content, so conditioning is essential for reproducible and comparable results.
Testing Items
A complete transverse ring crush index evaluation typically reports the following measured and calculated quantities:
- Transverse ring crush force, in newtons (N), for each individual specimen
- Transverse ring crush strength, in kN/m, averaged over all valid specimens
- Grammage of the sample, in g/m², determined in parallel according to ISO 536
- Transverse ring crush index, in N·m/g, calculated as ring crush strength divided by grammage
- Statistical information including mean value, standard deviation, coefficient of variation, and the number of valid tests
- Evaluation of the result against grade-specific minimum requirements where a product specification, such as GB/T 13023, applies
Testing Methods
Apparatus
The test requires a calibrated compression tester fitted with a standard ring crush holder assembly, which consists of a lower ring pedestal and an upper collar that curl the flat strip into a rigid circular cylinder. The tester operates at a constant compression speed, typically 12.5 mm/min, with parallel platens and a force measurement accuracy appropriate to the expected load range. The holder must be clean, undamaged, and periodically verified, because wear or debris in the holder seat is a common source of low or scattered results.
Test Procedure
The general sequence of the test is as follows:
- Verify the calibration status of the load cell and the geometry of the ring holder before starting the test series
- Insert a conditioned strip into the holder so that it forms a complete ring with the ends meeting without overlap or gap, taking care not to touch or damage the exposed test zone
- Place the holder assembly centrally between the platens, clear of the platen edges
- Apply compression at the specified constant speed until the specimen collapses, and record the maximum force
- Repeat the test for at least ten valid cross-direction specimens; discard and replace any specimen that slips in the holder, fails at the holder edge, or fails in an abnormal mode
- Determine the grammage of the matched specimens and calculate the reported quantities
Calculation and Expression of Results
The transverse ring crush strength is calculated by dividing the mean maximum force by the effective tested circumference of 152 mm, and the index is then obtained by normalizing the strength with grammage. For example, if a 120 g/m² medium yields a mean maximum force of 122 N, the ring crush strength is 122 / 0.152 = 0.80 kN/m, and the transverse ring crush index is 800 / 120 = 6.7 N·m/g. Results are reported to the standard number of significant figures, together with the conditioning atmosphere, number of specimens, and any deviations from the standard method.
Precision and Influencing Factors
Ring crush results are influenced by moisture content, cutting quality of the strip edges, holder condition, platen parallelism, and operator handling technique. Interlaboratory studies show that careful control of conditioning and holder maintenance significantly reduces variability. When disputes arise in trade, testing is normally repeated at accredited third-party laboratories under strictly standardized conditions.
Applications
Transverse ring crush index testing is used throughout the paper and packaging value chain for the following purposes:
- Mill quality control and grade certification, verifying that production lots meet the minimum index values defined in product standards such as GB/T 13023
- Incoming inspection at corrugating and box plants, ensuring that purchased medium will deliver the target board performance
- Product development and lightweighting programs, where higher index values allow grammage reductions without sacrificing box compression strength
- Prediction of downstream performance, since transverse ring crush data feed empirical models linking component properties to board ECT and box stacking strength
- Commercial acceptance and arbitration, with comparative testing performed by accredited third-party laboratories when suppliers and buyers disagree on quality
FAQ
Why is the ring crush test for corrugating medium performed in the cross direction?
When medium is fluted, the paper's cross direction follows the flute contour, so the medium carries vertical stacking loads as a series of arches oriented in the cross direction. The transverse ring crush index therefore reflects the direction of loading that actually governs board and box performance, which is why product standards specify the transverse value.
What is the difference between ring crush strength and ring crush index?
Ring crush strength is the maximum edgewise compressive force per unit length, expressed in kN/m. The ring crush index is the strength divided by grammage, expressed in N·m/g. The index removes the effect of basis weight so that the intrinsic compression quality of papers with different grammages can be compared directly.
How does the ring crush test differ from short-span compression testing?
The ring crush test supports the specimen in a circular holder and typically involves a longer unsupported span, making it sensitive to buckling behavior, while short-span compression (SCT) measures compression strength over a very short gauge length of 0.7 mm with minimal buckling influence. Both are used for containerboard, but the ring crush index remains the contractually specified property for corrugating medium in many markets.
What transverse ring crush index values are typical for corrugating medium?
Values depend strongly on furnish and grade. Ordinary recycled medium typically achieves roughly 4.5 to 6.5 N·m/g, while semi-chemical and high-strength grades commonly reach 7 to 9 N·m/g or higher. The applicable acceptance limits for a given basis weight and grade are defined in the product specification, such as GB/T 13023.
How many specimens are required and how should results be reported?
At least ten valid cross-direction specimens should be tested, taken from multiple positions across the web. The report should include the mean ring crush strength, grammage, calculated index, number of tests, conditioning atmosphere, and any specimens discarded due to invalid failure modes.
Can the same method be applied to linerboard and other paper grades?
Yes. The ring crush method per ISO 12192 and GB/T 2679.8 applies broadly to paper and board within the applicable thickness range, including linerboard and other packaging grades. For corrugating medium specifically, the transverse ring crush index is the property cited in product standards and commercial contracts.
Why Choose ZKGX?
- State-of-the-art analytical equipment
- Highly qualified scientific team
- Fast turnaround time
- Competitive pricing