Overlap length determination is a critical quality-control element in X-ray film radiographic testing, ensuring that successive exposures provide complete, gap-free coverage of welds and components that exceed the size of a single film. This article explains the technical principles, calculation procedures, marker-based verification methods, and applicable standards—such as ISO 17636-1, ASME BPVC Section V, and GB/T 3323—used by accredited third-party laboratories to quantify and validate overlap in industrial radiography.
Technical Overview
Film radiographic testing (RT) is one of the most established non-destructive testing methods for detecting internal discontinuities such as porosity, slag inclusions, lack of fusion, and cracks in welded joints and cast components. When the area to be inspected is larger than the usable area of a single film, the examination must be divided into a series of sequential exposures. Each adjacent pair of exposures must physically overlap so that no portion of the component escapes inspection.
The overlap length is the longitudinal distance along the weld or component covered by two neighboring film sections. Determining this length correctly involves two complementary activities: a geometric calculation performed before exposure, and a marker-based verification performed on the processed radiographs. High-density markers (typically lead characters or arrows) are positioned at the boundary of each exposure zone; if the marker image appears on both adjacent films, continuous coverage is demonstrated. If it is missing from either film, the gap between exposures was insufficient and the affected section must be re-radiographed.
The principal standards governing this practice include:
- ISO 17636-1 — Non-destructive testing of welds, radiographic testing, X- and gamma-ray techniques with film
- ASME Boiler and Pressure Vessel Code, Section V, Article 2 — Radiographic Examination
- GB/T 3323.1 — Chinese national standard for radiographic testing of fusion-welded joints
- ASTM E94 — Standard Guide for Radiographic Examination
- ASTM E1742 — Standard Practice for Radiographic Examination
- ISO 11699-1 and ISO 11699-2 — Classification of industrial radiographic film and film processing
Testing Samples
Butt-Welded Plate Assemblies
Long structural seams in plate and sheet material are the most common specimens requiring overlap determination. Because a single film (for example, 100 mm × 300 mm or 100 mm × 480 mm) covers only a fraction of a multi-meter seam, technicians must calculate the exposure spacing so that every segment of the weld is captured on at least one film at the specified density.
Pipe and Tube Girth Welds
Circumferential welds in pipes are examined using single-wall, double-wall, or panoramic techniques depending on diameter and accessibility. For these components, overlap length determination extends to computing the minimum number of exposures required to cover the full circumference, with film strips arranged end-to-end with a defined overlap zone.
Pressure Vessel and Boiler Seams
Longitudinal and circumferential seams in pressure equipment are typically examined in segments. Overlap verification is mandatory for code compliance, since an undetected gap in coverage could allow a rejectable discontinuity to escape evaluation.
Castings and Complex Components
Large castings with extensive areas of interest may require multiple overlapping exposures to demonstrate complete volumetric coverage of designated zones, particularly at section transitions and flange connections.
Testing Items
A complete overlap length determination program within an accredited third-party laboratory typically includes the following verification items:
- Calculation of usable film length after deducting edge trim zones and unqualified image areas
- Calculation of the minimum overlap length between adjacent exposures
- Placement and positional verification of overlap (lead) markers on the source side of the component
- Determination of the required number of exposures for circumferential welds
- Verification that overlap marker images appear on both adjacent processed radiographs
- Verification that optical density in the overlap region falls within the range permitted by the applied code
- Confirmation that no portion of the zone of interest is missing from the film set
Testing Methods
Principle of Overlap Determination
The method rests on a simple geometric fact: radiation diverges from the focal spot, so the projected boundary of an exposure does not coincide exactly with the film edge. Parallax, film edge fog, and marker placement tolerance all create a narrow zone of uncertainty at the boundary of each exposure. The overlap length compensates for this uncertainty. In general practice, the overlap is set to the greater of a fixed minimum value (commonly 10 mm, consistent with GB/T 3323 practice) or a calculated parallax-based value derived from the source offset and the source-to-film distance.
Establishing the Usable Film Length
The technician first determines the effective (usable) length of the film. This equals the physical film length minus the edge zones, where density gradients and clipped geometry make evaluation unreliable. The usable length is further limited by geometric requirements, including the maximum permitted geometric unsharpness Ug, calculated as Ug = f × b / (F − b), where f is the focal spot size, b is the object-to-film distance, and F is the source-to-film distance. For welds, the transverse thickness ratio K (the ray-path length through the wall relative to the nominal path) also constrains the usable arc or length per exposure; ISO 17636-1, for example, limits K to approximately 1.1 for Class A techniques on circumferential welds.
Calculating the Minimum Overlap Length
For a flat weld examined in sequential exposures, the required overlap accounts for the potential lateral misalignment between the source position and the film centerline. A conservative calculation doubles the maximum boundary shift produced by this offset and adds a fixed safety margin; in routine practice this is satisfied by adopting an overlap of at least 10 mm or approximately 10 percent of the usable film length, whichever is greater, unless the applied code specifies otherwise. The exposure pitch (center-to-center spacing of successive shots) is then set as the usable film length minus the overlap.
Placement of Overlap Markers
High-density markers—lead arrows, letters, or digits—are placed on the source side of the component at the calculated boundary of each exposure zone, on both sides of the weld where required. Source-side placement is essential: film-side markers do not correctly demonstrate coverage because parallax would move their shadows in the opposite direction to the true boundary. Marker height and thickness are selected so that the image remains visible above the background density without obscuring the weld.
Exposure Planning for Circumferential Welds
For girth welds examined by the double-wall single-image technique, the minimum number of exposures N is calculated by dividing the outer circumference by the usable transmittance arc length per exposure and rounding up to the next whole number. For panoramic (center-source) techniques, film strips are wrapped around the circumference with each adjacent pair overlapping by at least the specified minimum, allowing the entire weld to be examined in a single exposure. Elliptical techniques for small-bore tubes typically use two exposures offset by approximately 90 degrees, with overlap verification confirming that both halves of the joint are fully captured.
Verification on Processed Radiographs
After film processing, the inspector verifies three acceptance conditions on each adjacent film pair:
- The overlap marker image is visible on both films, demonstrating that the shared boundary zone was radiographed twice
- The optical density measured in the overlap region lies within the qualified range (for example, at least 2.0 for Class A and 2.3 for Class B per ISO 17636-1, or 1.8 to 4.0 for single-film viewing per ASME Section V)
- Weld features visible at the film edge on one radiograph continue seamlessly onto the adjacent radiograph, with no missing segment of the zone of interest
If any of these conditions is not met, the affected exposure is repeated with adjusted spacing until continuous coverage is demonstrated.
Equipment and Consumables
The determination relies on standard radiographic equipment: an X-ray generator of suitable energy for the material thickness, industrial film classified under ISO 11699-1 or ASTM E1815, lead intensifying screens, lead overlap markers, image quality indicators (wire or hole type) per ISO 19232 or ASTM E747/E1025, a calibrated densitometer, and a viewing illuminator of adequate luminance for evaluating maximum densities.
Applications
Overlap length determination is applied wherever film radiography must cover an inspection area larger than one film, including:
- Longitudinal and circumferential seam welds in pressure vessels, boilers, and storage tanks
- Girth welds in oil and gas pipelines and process piping systems
- Structural steel welds in bridges, buildings, and offshore platforms
- Welds in shipbuilding hulls and marine components
- Power plant components, including boiler tubes and header welds
- Castings, valve bodies, and pump casings in general manufacturing
- Aerospace and defense components requiring full volumetric coverage records
Documented overlap verification forms part of the permanent examination record, supporting traceability for fabrication codes, regulatory audits, and in-service integrity assessments.
FAQ
What is overlap length in film radiographic testing?
Overlap length is the linear distance along the weld or component that is captured on two adjacent film sections. It ensures that the boundary between successive exposures is examined at least twice, eliminating the possibility of an uninspected gap between exposures.
Why must overlap markers appear on both adjacent films?
The marker defines the calculated boundary of each exposure. If its image appears on both radiographs, the boundary zone was covered twice, proving continuous coverage. If it appears on only one film, a gap may exist and the exposure must be repeated.
What minimum overlap length is typically required?
Common practice, consistent with GB/T 3323 and widely adopted laboratory procedures, sets a minimum overlap of 10 mm between adjacent films. Codes such as ISO 17636-1 instead express the requirement functionally: the overlap must ensure the zone of interest appears completely on at least one film at the correct density, verified by markers appearing on both film sections.
How many exposures are needed to cover a girth weld?
The number equals the pipe outer circumference divided by the usable arc length per exposure, rounded up to the next whole number. When a panoramic technique with a centrally positioned source is feasible, a single exposure can cover the full circumference, provided the film strips around the circumference overlap by at least the specified minimum.
What happens if the overlap marker is missing on one film?
The film pair is rejected for coverage purposes. The technician repeats the exposure with reduced shot spacing (increased overlap) until both adjacent radiographs display the marker image and density requirements are satisfied.
Must the overlap region meet density and image quality requirements?
Yes. The overlap zone is part of the evaluated area, so its optical density must fall within the code-specified range and image quality indicators placed in the exposure must meet the required sensitivity. A visible marker alone does not compensate for under- or over-exposure in the overlap region.
Why Choose ZKGX?
- State-of-the-art analytical equipment
- Highly qualified scientific team
- Fast turnaround time
- Competitive pricing